Ohio Game Fishing banner

Enviro-Tex Help

1 reading
1.3K views 7 replies 6 participants last post by  All Eyes  
#1 ·
My E-Tex resin is turning white and crystalizing in the bottle. It looks like it's mixed with sugar. I am talking about un-used resin in a sealed bottle kept indoors and less than a year old. The hardener seems fine. Is this resin now junk, or can it be warmed or stirred somehow? The only thing I can think of is that there must be air getting into the bottle somehow by a pin hole or crack in the cap??? Has anyone experienced this problem?
 
#2 ·
Eyes,

No worries, it will crystalize when stored at low temps or on my basement concrete floor :D
microwave some water and sit her in a warm water bath and she will be fine, may take a couple rounds and tilts up and down...not sure at what temp the crash goes back into solution but it will.

Best,

MS
 
#6 ·
muskyslayer hit it on the head. The rod building epoxy I use most often is repackaged E-Tex with UV inhibitors (EX-74, I think). You can use the microwave, a warm bath, or set it on a candle warmer for a while. It takes a little time for the crystals to go away, and don't mix a batch before they are gone. I got a little aggressive one time and mixed a batch before the resin cleared, and had to toss it out.

Joe
 
#7 ·
I have had this problem over the years, now that I don't make as many baits as I used to I buy the smaller bottles, I have done the heating method it works, the only problem I have had at times if the humidity is high baits will dry sticky, most epoxy based resins are effected by moisture so I run a dehumidifier in the summer to dry the air at least 2 days before coating..